Abstrait:

The micromechanical properties of the steel-fiber-reinforced cementitious composites with different water-binder ratios and silica fume contents were studied by nanoindentation. The elastic modulus, indentation hardness, total input energy, and ratio of the elastic deformation energy to the total input energy were analyzed in the interfacial transition zone (ITZ) and the cement matrix. The results show that with the reduction of water-binder ratio in the range of 0.18–0.24, the elastic modulus, indentation hardness, elastic deformation capacity, and energy dissipation capacity increased in the ITZ and cement matrix, and the increase of the ITZ was greater than that of the matrix, yet the ITZ did not disappear. With the increase of silica fume content in the range of 0–30%, the weak ITZ was gradually strengthened or even disappeared. In terms of obtaining the stronger ITZ, adding silica fume is more effective than reducing the water-binder ratio. When the water-binder ratio was high at 0.24, large silica fume contents (30%) had significant effects on enhancing the micromechanical properties of the ITZ and matrix. At a low water-binder ratio of 0.18, large silica fume contents (30%) enhanced the micromechanical properties of the ITZ while degrading those of the cement matrix.

Copyright: © 2021 Yan-Ru Zhao et al.
License:

Cette oeuvre a été publiée sous la license Creative Commons Attribution 4.0 (CC-BY 4.0). Il est autorisé de partager et adapter l'oeuvre tant que l'auteur est crédité et la license est indiquée (avec le lien ci-dessus). Vous devez aussi indiquer si des changements on été fait vis-à-vis de l'original.

  • Informations
    sur cette fiche
  • Reference-ID
    10555042
  • Publié(e) le:
    22.01.2021
  • Modifié(e) le:
    02.06.2021
 
Structurae coopère avec
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine